1
Sand the surface
Sanding deeply with grit P200-P400 sandpaper
wetly.
2
Spray 2K04 Surfacer
Spray 2 – 3 coats of 2K04 surfacer with
5–8-minute interval (or longer depending
on weather conditions).
3
Sand the surface smooth
Sanding smooth with grit P800 – P1000
sandpaper wetly until the surface feeling
smooth.
Tips: while sanding the sound of sanding got
lower when it is become finer.
Important Activation Information
Activation of 2k04 Epoxy Surfacer is important,
as non-proper activation may end with non-dry paint.
Use Time
4 hours after activating
Touch Dry
2 hours
Next Color Coat
2 hour waiting time is require before
the next color coat.
Interval Each Coat
5-8 minutes